Tellurium | |
Electron Configuration | 2,8,18,18,6 |
Electron Configuration | [Kr] 4d10 5s2 5p4 |
Ground state | 3P2 |
Atomic Volume | 20.5 g/cm3 |
Electronegativity | 2.1 |
Magnetic ordering | Non-magnetic |
Mass magnetic susceptibility | -3.9 x 10-9 |
Molar magnetic susceptibility | -4.98 x 10-10 |
Speed of sound | 2610 m s-1 |
Thermal Properties | |
Enthalpy of Atomization | 190.4 kJ mol-1 @25°C |
Enthalpy of Fusion | 13.5 kJ mol-1 |
Enthalpy of Vaporisation | 104.6 kJ mol-1 |
Heat Capacity | 25.73 J mol-1 K-1 |
Thermal Conductivity | 1.97 - 3.38 W m-1 K-1 |
Thermal Expansion | No data. |
Hardness | |
Brinell hardness | 180 MPa |
Mohs hardness | 2.25 |
Elastic Properties | |
Bulk modulus | 65 GPa |
Shear modulus | 16 GPa |
Young's modulus | 43 GPa |
Electrical Properties | |
Electrical resistivity | No data. |
Electrical conductivity | No data. |
Chemical Properties | |
Electrochemical Equivalent | 1.1902 g Ah-1 |
Electron Work Function | 4.95 eV |
Valence Electron Potential (-eV) | 59 |
Ionization Potential | |
First | 9.009 |
Second | 18.6 |
Third | 27.96 |
Incompatibilities | Oxidizers, chlorine, cadmium. |
Flammability | |
Combustible Solid |
Optical Properties | |
Refractive Index (gas) | 1.000991 |
Reflectivity | % |
Energy Levels | |
Kα1 (intensity 100) | 27.4723 KeV |
Kα2 (intensity 50) | 27.2017 KeV |
Kβ1 (intensity 19.7) | 30.9957 KeV |
Kβ2 (intensity 5.7) | 31.6947 KeV |
Kβ3 (intensity 8.6) | 30.9388 KeV |
Lα1 (intensity 100) | 3.76933 KeV |
Lα2 (intensity 10) | 3.7588 KeV |
Lβ1 (intensity 51.3) | 4.02958 KeV |
Lβ2 (intensity 16.3) | 4.3017 KeV |
Lβ3 (intensity 5.8) | 4.1192 KeV |
Lβ4 (intensity 4) | 4.0684 KeV |
Lγ1 (intensity 5.6) | 4.5709 KeV |
Lγ2 (intensity 2) | 4.8253 KeV |
Lγ3 (intensity 2) | 3.604 KeV |
Ll (intensity 4.5) | 3.3344 KeV |
Atomic Radii | |
Empirical | 140 pm |
Bohr Radius | 123 pm |
Covalent Radius | 135 pm |
Van der Waals | 206 pm |
Triple covalent | 121 pm |
Metallic | No data. |
Ionic Radii (Å) | ||||
Charge | Coordination | Crystal | Ionic | Key |
-2 | VI | 2.07 | 2.21 | P |
4 | III | 0.66 | 0.52 | |
IV | 0.8 | 0.66 | ||
VI | 1.11 | 0.97 | ||
6 | IV | 0.57 | 0.43 | C |
VI | 0.7 | 0.56 | * |
R, From r3 vs V plots. |
C, Calculated from bond length - bond strength equations. |
E, Estimated. |
*, Most Reliable. |
M, From Metallic Oxides. |
A, Ahrens (1952) Ionic radius. |
P, Pauling's (1960) Crystal Radius. |
Oxidation States | |
Main | Te+4 |
Other | Te-2, Te-1, Te0, Te+2, Te+5, Te+6 |
Ionisation Energies (kJ mol-1) | |
M - M+ | 869.2 |
M+ - M2+ | 1795 |
M2+ - M3+ | 2698 |
M3+ - M4+ | 3610 |
M4+ - M5+ | 5668 |
M5+ - M6+ | 6822 |
M6+ - M7+ | 13200 |
M7+ - M8+ | 15800 |
M8+ - M9+ | 18500 |
M9+ - M10+ | 21200 |
Covalent Bonds (kJ mol-1) | |
Te-H | 240 |
Te-O | 268 |
Te-F | 335 |
Te-Cl | 251 |
Te-Te | 235 |
Vapour Pressure | ||||||
P (Pa) | 1 | 10 | 100 | 1K | 10K | 100K |
T (K) | (775) | (888) | 1042 | 1266 | ||
Crystal Structure | |
Structure | Trigonal |
a = 445.72 pm | |
b = 445.72 pm | |
c = 592.9 pm | |
α = 90° | |
β = 90° | |
γ = 120° |